(1): the extrusion coefficient of aluminum profile is too large, the extrusion temperature is too high (bar, tube, die three temperature), the extrusion speed is too fast.
(2): the extrusion pressure is unstable, suddenly high and suddenly low, or the speed difference between multi-speed regulation is obvious, the speed conversion is fast when changing gears.
(3): aluminum alloy profile extrusion head end pressure (stamping) too fast, tail end running speed or not decelerated, a lot of infiltration of the dead zone of aluminum.
(4) the quality of the rod is poor, the rod is over-burned, with large grains and loose. Residual pressure (V3 aluminum) is too thin.
(5): extrusion die velocity ratio serious imbalance unreasonable design and manufacturing.
Previous:Switch aluminum plate drilling often appear problems
Next:Related factors that affect the quality of aluminum coil |
Back to list |
How to quickly identify inferior aluminum?
2019-08-27Performance of aluminum oxide plate
2019-08-27What's the difference between tin foil and aluminum foil?
2019-08-27Related factors that affect the quality of aluminum coil
2019-08-27Causes of surface cracks in aluminum profiles
2019-08-27Switch aluminum plate drilling often appear problems
2019-08-27